The electrical properties of poly(3,4-et ...
Type de document :
Article dans une revue scientifique: Article original
DOI :
URL permanente :
Titre :
The electrical properties of poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate) films and its effect onto sensor yarn coating
Auteur(s) :
Jerkovic, Ivona [Auteur]
Grancaric, A. M. [Auteur]
Koncar, Vladan [Auteur]
Génie et Matériaux Textiles [GEMTEX]
Grancaric, A. M. [Auteur]
Koncar, Vladan [Auteur]
Génie et Matériaux Textiles [GEMTEX]
Titre de la revue :
Journal of Industrial Textiles
Nom court de la revue :
J. Ind. Text.
Numéro :
51
Pagination :
8549S-8564S
Éditeur :
SAGE Publications
Date de publication :
2020-05-21
ISSN :
1528-0837
Mot(s)-clé(s) en anglais :
Smart textiles
polymer formation
chemistry
coatings
fiber
yarn
fabric formation
fabrication
polymer formation
chemistry
coatings
fiber
yarn
fabric formation
fabrication
Discipline(s) HAL :
Sciences de l'ingénieur [physics]
Résumé en anglais : [en]
In this study, the poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate) conductive dry films were observed in terms of their thicknesses versus electrical resistances measured and related electrical resistivities ...
Lire la suite >In this study, the poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate) conductive dry films were observed in terms of their thicknesses versus electrical resistances measured and related electrical resistivities calculated. The evolution of their electrical resistances was monitored in 75 days. Three groups of sensor yarns were studied also where the percolation threshold of the polymer complex poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate) had a crucial role in their manufacture. More glass component in sensor yarns led to less coating thickness what is in correlation with their interface phenomena and adhesion.Lire moins >
Lire la suite >In this study, the poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate) conductive dry films were observed in terms of their thicknesses versus electrical resistances measured and related electrical resistivities calculated. The evolution of their electrical resistances was monitored in 75 days. Three groups of sensor yarns were studied also where the percolation threshold of the polymer complex poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate) had a crucial role in their manufacture. More glass component in sensor yarns led to less coating thickness what is in correlation with their interface phenomena and adhesion.Lire moins >
Langue :
Anglais
Audience :
Internationale
Vulgarisation :
Non
Établissement(s) :
Université de Lille
ENSAIT
Junia HEI
ENSAIT
Junia HEI
Collections :
Date de dépôt :
2023-06-20T11:31:46Z
2024-03-15T14:41:48Z
2024-03-15T14:41:48Z